ABSTRACT:
Process for improving the crack growth behavior of titanium alloys containing substantial beta stabilizers and at least 3% molybdenum, such as Ti-6-2-4-6. The process includes the steps of forging above the beta transus temperature, cooling at a controlled rate through the beta transus temperature, heating to a temperature between 50.degree.-150.degree. F. below the beta transus temperature, cooling the alloy at a rate in excess of that produced by air cooling, and aging the material between about 900.degree. F. and 1100.degree. F. The resultant material has substantially improved crack growth behavior when contrasted with material processed according to the prior art.
REFERENCES:
patent: 3748194 (1973-07-01), Ruckle et al.
patent: 4053330 (1977-10-01), Henricks et al.
patent: 4309226 (1982-01-01), Chen
Berczik Douglas M.
Brodi George
O'Connell Thomas E.
Sohl Charles E.
Stallard Wayland W.
United Technologies Corporation
LandOfFree
Processing for titanium alloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Processing for titanium alloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Processing for titanium alloys will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1612561