ABSTRACT:
A water dispersion comprising i) up to about 50% by weight of a water-dispersible low molecular weight polyester having a number average molecular weight in the range of about 850-2500 and preferably 1100-1800 and an acid value in the range of about 40-85 milligrams of KOH/gram of said polyester (millig/g) and preferably in the range of about 45-65 millig/g, which comprises: (1) a non-linear polyester backbone having an acid value in the range of about 5-15 millig/g and preferably about 8-12 millig/g comprising the reaction product of an aliphatic polyol, an aromatic dicarboxylic acid, and a monocarboxylic acid and (2) pendant moieties of a polycarboxylic acid having at least one free carboxylic acid group and at least one ester linkage to said backbone, ii) about 0.5% to 4% by weight, as based upon said polyester, of a chelated titanate, and iii) a fugitive base, is disclosed to provide a useful warp sizing composition for synthetic yarn fibers.

REFERENCES:
patent: 2334107 (1943-11-01), Light et al.
patent: 2378230 (1945-01-01), Little
patent: 3734874 (1973-05-01), Kibler et al.
patent: 3779993 (1973-12-01), Kibler et al.
patent: 3853820 (1974-12-01), Vachon
patent: 4016330 (1977-04-01), Laganis
patent: 4035531 (1977-07-01), Lark
patent: 4066593 (1978-01-01), Czajka et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process of warp sizing which uses a low molecular weight polyest does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process of warp sizing which uses a low molecular weight polyest, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process of warp sizing which uses a low molecular weight polyest will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-221438

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.