Process of making polyurethane elastomer thread

Plastic and nonmetallic article shaping or treating: processes – Forming continuous or indefinite length work – Shaping by extrusion

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

26421114, 2642905, 528 76, 528 80, 528 83, D01D 5092, D01D 516, D01F 670

Patent

active

053624335

ABSTRACT:
In a process for producing melt-spun elastomer threads with a high modulus, a breaking elongation of 80 to 300% and a boiling shrinkage of at least 20%, multifilament elastic threads are obtained by spin-drawing. A molten mass of polyurethane granulate is simultaneously drawn at a drawing factor of at least 1.5 and wound on spools at 600 m/min. or more. The spun-drawn, non-adhesive TPU thread can be processed to form a flat structure, the elasticity of which can be regulated by setting or by tempering in hot water. The thread can also be tempered before being processed in order to acquire the desired elastic properties.

REFERENCES:
patent: 3536803 (1970-10-01), Epstein et al.
patent: 3663677 (1972-05-01), Keuchel
patent: 3679633 (1972-07-01), Matsubayashi et al.
patent: 3686387 (1972-08-01), Keberle et al.
patent: 4751139 (1988-06-01), Hensel et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process of making polyurethane elastomer thread does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process of making polyurethane elastomer thread, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process of making polyurethane elastomer thread will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1780193

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.