ABSTRACT:
High-strength polyvinyl alcohol fiber is provided by extruding a polyvinyl alcohol dope solution through a spinneret into a coagulating bath, the spinneret being located such that substantially only its dope-extruding surface contacts the coagulating bath. This process can produce stably and at a low cost polyvinyl alcohol fibers with excellent strength.
Naramura Syunpei
Ohmory Akio
Sano Hirofumi
Sano Tomoyuki
Yoshimochi Hayami
Kuraray Co. Ltd.
Tentoni Leo B.
LandOfFree
Process of making high-strength polyvinyl alcohol fiber does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process of making high-strength polyvinyl alcohol fiber, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process of making high-strength polyvinyl alcohol fiber will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1758537