ABSTRACT:
In amorphous silicon nitride powder, from 0.5 to 40 mol % of the silicon are replaced by one or more of the elements boron, aluminum, yttrium, lanthanum, titanium, zirconium, tungsten and molybdenum.
The powder is obtained by reacting the halides of the corresponding elements, which are dissolved in an inert organic solvent in the particular ratio desired, with ammonia. The solid reaction product formed is separated off from the liquid phase and treated at from 800.degree. to 100.degree. C.
The powder is particularly suitable as a starting material for the production of sintered articles.
REFERENCES:
patent: 4145224 (1979-03-01), Mehalchick et al.
patent: 4196178 (1980-04-01), Iwai et al.
patent: 4517168 (1985-05-01), Kawahito et al.
patent: 4734234 (1988-03-01), Sterzel
BASF - Aktiengesellschaft
Dixon Jr. William R.
Group Karl
LandOfFree
Process of making amorphous silicon nitride powder does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process of making amorphous silicon nitride powder, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process of making amorphous silicon nitride powder will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2417694