Process of making a non-corrosive GMR slider for proximity...

Metal working – Method of mechanical manufacture – Electrical device making

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C029S603120, C029S603130, C029S090010, C428S827000, C428S828000

Reexamination Certificate

active

10783678

ABSTRACT:
A method of fabrication of a slider includes forming a first ferromagnetic layer, a second ferromagnetic layer, and an antiferromagnetic layer and applying a layer of protective material to proximal ends of those layers that are proximal to the disk surface. The method further includes recessing a proximal end of a non-magnetic metal layer formed on the first ferromagnetic layer from the disk surface to form at least one recessed area. The method also includes filling the recessed area with protective material to a depth such that when the layer of protective material is worn from the ends of the first ferromagnetic layer, the second ferromagnetic layer, and the antiferromagnetic layer by burnishing of the ends by the disk surface, protective material still remains in the recessed area of the non-magnetic metal layer.

REFERENCES:
patent: 4188247 (1980-02-01), Ridgway et al.
patent: RE32464 (1987-07-01), Aine
patent: 4948460 (1990-08-01), Sandaiji et al.
patent: 5003688 (1991-04-01), Terada et al.
patent: 5013394 (1991-05-01), Rolland et al.
patent: 5608593 (1997-03-01), Kim et al.
patent: 5667879 (1997-09-01), Haji-Sheikh
patent: 5696654 (1997-12-01), Gill et al.
patent: 5735036 (1998-04-01), Barr et al.
patent: 5761790 (1998-06-01), Carr et al.
patent: 5766743 (1998-06-01), Fujikata et al.
patent: 5777824 (1998-07-01), Gray
patent: 5805380 (1998-09-01), Ishihara et al.
patent: 5822153 (1998-10-01), Lairson et al.
patent: 5901431 (1999-05-01), Santini
patent: 5903969 (1999-05-01), Haga
patent: 5943187 (1999-08-01), Chen et al.
patent: 5986851 (1999-11-01), Angelo et al.
patent: 5991119 (1999-11-01), Boutaghou et al.
patent: 5999380 (1999-12-01), Slade et al.
patent: 6201669 (2001-03-01), Kakihara
patent: 6282043 (2001-08-01), Korenari
patent: 6324747 (2001-12-01), Boutaghou et al.
patent: 6369993 (2002-04-01), Hayashi
patent: 6427319 (2002-08-01), Cook et al.
patent: 6493179 (2002-12-01), Kohira et al.
patent: 6493193 (2002-12-01), Honma et al.
patent: 6721142 (2004-04-01), Meyer et al.
patent: 2003/0099069 (2003-05-01), Kagami et al.
patent: 57-108265 (1982-07-01), None
Sbiaa et al., “Ferro- and Antiferromagnetic Exchange Coupling in Magnetooptical Bilayers with Planar and Perpendicular Anisotropy”, IEEE Transactions on Magnetics, vol. 31., No. 6, Nov. 1995, pp. 3274-3276.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process of making a non-corrosive GMR slider for proximity... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process of making a non-corrosive GMR slider for proximity..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process of making a non-corrosive GMR slider for proximity... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3826835

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.