Process for welding nickel-based superalloys

Electric heating – Metal heating – By arc

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

2191218, 21912184, 427 531, 427432, B23K 2600

Patent

active

048048151

ABSTRACT:
A process for preventing crack formation in nickel alloy substrates having a gamma-prime phase includes providing a substrate comprised of a nickel alloy having a gamma-prime phase. A portion of the substrate is irradiated with a laser beam and thereby forms a molten pool of the alloy. A supply of coating particles are dispersed within the pool, the particles are comprised of a nickel alloy having gamma-prime forming constitutents. Rapid relative motion between the beam and the pool is effected so that the pool rapidly solidifies and thereby minimizes the formation of gamma-prime therein and adjacent thereto.

REFERENCES:
patent: 4117302 (1978-09-01), Earle et al.
patent: 4269868 (1981-05-01), Livsey
patent: 4299860 (1981-11-01), Schaefer et al.
patent: 4300474 (1981-11-01), Livsey
patent: 4323756 (1982-04-01), Brown et al.
patent: 4533815 (1985-08-01), Ecer
patent: 4615903 (1986-10-01), Miller
patent: 4730093 (1988-03-01), Mehte et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for welding nickel-based superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for welding nickel-based superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for welding nickel-based superalloys will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1367082

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.