ABSTRACT:
A continuous process for extraction of niobium, rare earths and thorium from niobium ore concentrates which includes digesting the ore with a hot solution containing 13 to 16 moles of sulphuric acid per liter, diluting the solution to a concentration of 10 to 13 moles of sulphuric acid per liter, separating the insolubles from the solution which includes alkaline earth sulphates and the sulphates of thorium and rare earths that are present, reducing titanium in solution to the trivalent state and diluting the solution to a concentration of 5 to 7 moles of sulphuric acid per liter, separating the precipitated niobium oxide and sulphates of thorium and rare earths, and then concentrating the resulting solution to the level desired for recycle to the digestion stage.

REFERENCES:
patent: 2885259 (1959-05-01), McCullough
patent: 2932555 (1960-04-01), Flynn

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for treatment of pyrochlore concentrates does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for treatment of pyrochlore concentrates, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for treatment of pyrochlore concentrates will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-521535

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.