ABSTRACT:
A process for treating molten cast iron in an open ladle by means of pure magnesium is proposed, wherein the pure magnesium is introduced in a multiplicity of very small magnesium particles, coated with a protective layer, into the molten cast iron.
The protective layer, which protects the magnesium from premature melting and controls the reaction rate, is produced from ceramics.
The process can be carried out with very simple equipment. Involved pretreatments of the treatment agent are unnecessary.
REFERENCES:
patent: 3957502 (1976-05-01), Cull
patent: 4040818 (1977-08-01), Clegg
patent: 4364771 (1982-12-01), Cordier
patent: 4541867 (1985-09-01), Neelameggham
patent: 4592777 (1986-06-01), Rellermeyer
Gut Karl
Henych Ivo
Georg Fischer AG
Rosenberg Peter D.
LandOfFree
Process for treating molten cast iron in an open ladle by means does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for treating molten cast iron in an open ladle by means , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for treating molten cast iron in an open ladle by means will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1922640