ABSTRACT:
For protecting iron sponge particles against reoxidation and/or corrosion a coating comprising CaO as well as iron or iron oxides as adhesion promotor is applied onto the iron sponge particles. Water is subsequently sprayed onto this coating whereupon a second coating of a mixture of dust-shaped CaO and a carbon carrier is applied. This second coating is subsequently humidified with a smaller amount of water than would be necessary for completely slaking the CaO contained within the second coating.
REFERENCES:
patent: 3690930 (1972-09-01), Mueller
patent: 4075370 (1978-02-01), Burlengam
patent: 4254167 (1981-03-01), Sulzbecher
patent: 4290800 (1981-09-01), Sensis
Saiger Gunther
Stift Kurt
Sulzbacher Horst
Silverberg Sam
Voest-Alpine Aktiengesellschaft
LandOfFree
Process for treating metallic starting materials for smelting pl does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for treating metallic starting materials for smelting pl, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for treating metallic starting materials for smelting pl will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1734451