Process for the stabilization of copolymers of maleic anhydride

Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – Treating polymer containing material or treating a solid...

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

526272, C08F 628

Patent

active

053409183

ABSTRACT:
A copolymer of maleic anhydride and an alkyl vinyl ether is stabilized by contacting same with a non-reactive substantially moisture free gas at a temperature of from about 30.degree.-100.degree. C. for from about 0.5-24 hours. The copolymer is preferably prepared by reacting together maleic anhydride and an alkyl vinyl ether in the presence of a free radical initiator.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for the stabilization of copolymers of maleic anhydride does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for the stabilization of copolymers of maleic anhydride , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for the stabilization of copolymers of maleic anhydride will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-503968

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.