ABSTRACT:
In a process for the recovery of an atactic polymer which comprises heating liquid propylene containing the dissolved atactic polymer at a gauge pressure of 13 to 40 kg/cm.sup.2 in a vaporizer to vaporize the propylene, and separating the atactic polymer from the vaporized propylene thereby recovering the polymer in a molten state, the improvement comprising maintaining the vaporization temperature of propylene at 45.degree. C. to 90.degree. C. and the temperature of a heating medium for the vaporizer at 60.degree. C. to 150.degree. C. According to this process, a long run can be used in the recovery of the atactic polymer.

REFERENCES:
patent: 3644583 (1972-02-01), Scoggin

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for the recovery of atactic polymers does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for the recovery of atactic polymers, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for the recovery of atactic polymers will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-476008

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.