Process for the production of isotrophic spherical fuel or absor

Plastic and nonmetallic article shaping or treating: processes – Shaping or treating radioactive material

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

252637, 252639, 264 57, 264 60, 264 63, 264 65, 376411, 376412, 376414, 376419, 427 6, G21C 2102, G21C 302, C09K 1104

Patent

active

046684441

ABSTRACT:
Substantially isotropic spherical fuel and absorber elements for high temperature reactors are produced by molding corresponding fuel particles and graphite molding compositions. There is used as graphite molding powder a mixture of graphitized granules of coke and a hardenable resin binder. There are first produced in steel dies at 80.degree. to 120.degree. C. half shells and a nucleus with a pressed density of 1.0 to 1.4 g/cm.sup.3 followed by molding in a further steel die to the final format.

REFERENCES:
patent: 3978177 (1976-08-01), Huschka et al.
patent: 4022663 (1977-05-01), Hrovat et al.
patent: 4045526 (1977-08-01), Iwamoto et al.
patent: 4134941 (1979-01-01), Hrovat et al.
patent: 4140738 (1979-02-01), Hrovat et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for the production of isotrophic spherical fuel or absor does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for the production of isotrophic spherical fuel or absor, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for the production of isotrophic spherical fuel or absor will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-702491

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.