ABSTRACT:
Foamed plastics with improved combustion characteristics and good mechanical strength are obtained by condensation of aminoplast precondensates with organic isocyanates in the presence of an acid curing catalyst and an accelerator for polyurethane formation, whereby the precondensate used as starting material is prepared by reacting formaldehyde with urea and/or melamine in a molar ratio of 1.80 to 4.5:1 at pH values of 4 to 9.5, adjusting then the pH to 7.0 to 8.0 and adding urea to obtain a molar ratio offormaldehyde to the total amount of aminoplast forming compound of 1.0-2.1:1.

REFERENCES:
patent: 2806006 (1957-09-01), Proctor
patent: 3523093 (1970-08-01), Stomberger
patent: 3632531 (1972-01-01), Rush

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for the production of foamed plastics with improved comb does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for the production of foamed plastics with improved comb, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for the production of foamed plastics with improved comb will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2275136

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.