ABSTRACT:
The present invention relates to a continuous process for the production of impact resistance-modified thermoplastics. An elastomer, in particular a particulate graft polymer with a water moisture content of 1 to 50%, preferably 10 to 40%, is incorporated into a thermoplastics melt in a large volume kneader reactor. The mixing ratio of elastomer to thermoplastics melt is 4:1 to 1:4. The energy required to melt the elastomer and to evaporate the adhering water is added by heating the walls of the apparatus and via the kneading action of the installed rotating parts.
Liesenfelder Ulrich
Thiem Hans-Jurgen
Ullrich Martin
Bayer Aktiengesellschaft
Cain Edward J.
LandOfFree
Process for the production of elastomer-modified thermoplastics does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for the production of elastomer-modified thermoplastics, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for the production of elastomer-modified thermoplastics will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1726648