ABSTRACT:
The resistance of tableware decorations to cutlery abrasion traces can be increased by using, in the production of the decoration, a decoration coloring substance containing a pigment and a glass flux with the characteristics profile according to the invention: the pigment of the decoration coloring substance has an average grain diameter equal to or less than 2 .mu.m, and the glass flux of the decoration coloring substance has a density equal to or less than 2.6 g/cm.sup.3 and a hemisphere temperature less than 930.degree. C.

REFERENCES:
patent: 4446241 (1984-05-01), Francel et al.
patent: 5194089 (1993-03-01), Speer et al.
patent: 5238881 (1993-08-01), Norris et al.
patent: 5326728 (1994-07-01), Boury et al.
Volz, "Industrial Color Testing Fundamentals and Techniques", 1995, pp. 132-135.
Ullmann's Enzyklopadie der technischen Chemie, 4th Edition, vol. 14 (1977), pp. 9-10.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for the production of decorated tableware with increased does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for the production of decorated tableware with increased, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for the production of decorated tableware with increased will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-256663

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.