ABSTRACT:

FIELD OF THE INVENTION
The present invention relates to yttrium aluminum garnet fluorescent powders comprising a rare earth metal other than europium (Eu). The present invention also relates to the preparation of the yttrium aluminum garnet fluorescent powders and their use in a light-emitting device, particularly in a pink light-emitting device with high brightness.
BACKGROUND OF THE INVENTION
Conventional fluorescent powders for use in pink light-emitting diodes are mainly produced by adding europium into crystal compounds (also named main lattice) such as Y
3
Al
5
O
12
:Eu
3+
and Y
2
O
3
:Eu
3+
. Among them, yttrium aluminum garnet (YAG) has better light-emitting efficiency. The colors, i.e., chromaticity diagrams, of fluorescent powders can be controlled by changing the added amounts of europium. However, the variation range of color that can be controlled is small. II other words, it is difficult to control the concentration of the single luminescence center to obtain the desired chromaticity diagram.
Accordingly, fluorescent powders for pink light-emitting diodes without the above drawbacks and processes for the preparation of the fluorescent powders are highly desired.
SUMMARY OF THE INVENTION
The object of the present invention is to provide yttrium aluminum garnet fluorescent powders with formula (Y
3-x-y
Z
x
Eu
y
)Al
5
O
12
or (Y
3
Z
x
Eu
y
)Al
5
O
12
, wherein 0<x≦0.8, 0<y≦1.5, and Z is selected from a group consisting of rare earth metals other than europium (Eu).
Another object of the present invention is to provide a pink light-emitting device with high brightness, which comprises a visible or ultraviolet light-emitting diode as a luminescent element and a fluorescent body containing yttrium aluminum garnet fluorescent powders, wherein the diode emits a light with a wavelength ranging from 370 to 410 nm, and the light then excites the yttrium aluminum garnet fluorescent powders in the fluorescent body to emit another light with a wavelength ranging from 585 nm to 700 nm, so the two lights combine to produce a pink light with uniformly distributed colors.
Another object of the present invention is to provide a process for the preparation of the yttrium aluminum garnet fluorescent powders.


REFERENCES:
patent: 3699478 (1972-10-01), Pinnow et al.
patent: 6509651 (2003-01-01), Matsubara et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for the preparation of pink light-emitting diode... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for the preparation of pink light-emitting diode..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for the preparation of pink light-emitting diode... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3250151

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.