ABSTRACT:
A substantially stoichiometric mixture of calcic aluminate and calcium sulphate, as white as possible, formed at a temperature in the range of about 20.degree. to 90.degree. C, is hydrated simultaneously; water is added at least in stoichiometric proportions for the reaction and at a maximum in an amount such that after the reaction a product is obtained containing 5% (dry) ettringite and 95% (by weight) water, stoichiometry being defined, for example by the reaction

REFERENCES:
patent: 2248032 (1941-07-01), Dunn et al.
patent: 3391995 (1968-07-01), Rosenstock et al.
patent: 3565648 (1971-02-01), Mori et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for the manufacture of a fine white filler for industria does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for the manufacture of a fine white filler for industria, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for the manufacture of a fine white filler for industria will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1741466

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.