ABSTRACT:
Under specified conditions of reaction, a substantially pure aqueous solution of diallyldimethylammonium fluoride monomer can be polymerized to provide corresponding polymers having an intrinsic viscosity of at least about 0.1 deciliter per gram measured in 1.0 N NaCl solutions.

REFERENCES:
patent: 3288770 (1966-11-01), Butler
patent: 3514435 (1970-05-01), Ardis et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for the high molecular weight polymers of diallyldimethy does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for the high molecular weight polymers of diallyldimethy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for the high molecular weight polymers of diallyldimethy will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-600663

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.