Process for the dissolution of copper metal

Organic compounds -- part of the class 532-570 series – Organic compounds – Heavy metal containing

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

Reexamination Certificate

active

06646147

ABSTRACT:

BACKGROUND OF THE INVENTION
1. Field of the Invention
The present invention relates to a process for the dissolution of copper metal. More particularly, the invention relates to a process for producing a copper-containing aqueous solution by dissolving copper in the presence of an oxidant in an aqueous leach liquor containing monoethanolamine and (monoethanolammonium)
2
carbonate (HMEA)
2
CO
3
.
2. Description of the Prior Art
It is known to employ copper-containing aqueous solutions as biocidal fluids, for example, for the pressure treatment of lumber and for water purification. Examples of such fluids and uses thereof may be found, for example, in U.S. Pat. No. 4,929,454 and U.S. Pat. No. 6,294,071. The copper-containing solutions may be formulated, for example, by dissolving copper in aqueous solutions containing alkyl amines or alkyl hydroxy amines, such as 2-hydroxyethylamine.
Alternatively, copper-containing solutions may be produced by reacting copper oxide with chromic acid and arsenous acid to produce a solution of the copper with chrome and arsenic. The solution is subsequently diluted with water and the resulting aqueous solution may be injected into wood under pressure.
This chromated copper arsenate (“CCA”) is the primary additive used in the treatment of wood against termite and other biological infestation. Although the CCA is very effective, it has come under increased pressure because of the environmental concerns associated with chromium and arsenic.
A new generation of pesticide is now emerging that appears to be efficacious, and which relies on the use of copper (in larger quantities than in the CCA) in combination with other pesticidal components, such as quaternary amines and triazoles. The copper is typically applied as a solution of the monoethanolamine complex of copper carbonate or borate. The commercial form of the copper concentrate usually contains about 100 to 130 g/l copper which is diluted with water prior to injection into the wood.
The copper complex is typically produced commercially by the dissolution of basic copper carbonate in a solution of monoethanolamine (MEA), followed by further carbonation or addition of boric acid. The reactions can be approximately represented by the following equations:
CuCO
3
Cu(OH)
2
+7MEA→ Cu(MEA)
3.5
CO
3
+Cu(MEA)
3.5
(OH)
2
Cu(MEA)
3.5
(OH)
2
+CO
2
(or Boric acid)→ Cu(MEA)
3.5
CO
3
+H
2
O
The production of the copper carbonate precursor has its own production and raw material costs, and a brine waste is generated which gives rise to environmental concerns. A more efficient process might be to produce the complex without the aid of an isolated precursor. It is known from the prior art that ammonia and carbon dioxide in water can be used to dissolve copper metal with oxygen from air as the oxidant. This is represented by the following equation:
Cu+2NH
3
+(NH
4
)
2
CO
3
+1/2O
2→ Cu(NH
3
)
4
CO
3
+H
2
O
The reaction proceeds well and has been the basis for copper dissolution in several commercial facilities. However, if the ammonia is not initially carbonated, the kinetics are very poor which makes the process unattractive from a commercial standpoint.
A need exists for a more efficient process for producing copper-containing aqueous solutions, suitable for use in the wood-treatment industry. The present invention seeks to fill that need.
SUMMARY OF THE INVENTION
It has been discovered, according to the present invention, that it is possible to efficiently produce copper-containing solutions directly without initially producing or isolating a precursor such as copper carbonate. The present invention accordingly provides a process for producing a copper-containing aqueous solution, wherein a copper mass is dissolved in the presence of an oxidant in an aqueous leach liquor containing monoethanolamine and (monoethanolammonium)
2
carbonate (HMEA)
2
CO
3
, the leach liquor being produced by partially carbonating the monoethanolamine. According to the process, copper-containing solution may be produced in 8-12 hours or less, more usually within about 8 hours or less.


REFERENCES:
patent: 4929454 (1990-05-01), Findlay et al.
patent: 5084201 (1992-01-01), Greco
patent: 5304666 (1994-04-01), McLain
patent: 6294071 (2001-09-01), Miller et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for the dissolution of copper metal does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for the dissolution of copper metal, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for the dissolution of copper metal will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3183586

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.