ABSTRACT:
Modacrylic fibers having high retraction, reduced inflammability and high glossiness, prepared by wet spinning a solution, in an organic spinning solvent miscible with water, of a mixture of copolymers from acrylonitrile, vinylidene chloride, at least a vinyl ester and at least an unsaturated monomer containing at least a sulphonic group, the acrylonitrile units being from 50% to 85% by weight and the vinyl ester units from 3% to 6% by weight; hot drawing the coagulated fiber in a mixture of water and spinning solvent; drying the fiber in hot air while leaving it free concurrently to contract; and subsequently further hot drawing it in air.

REFERENCES:
patent: 3052512 (1962-09-01), Kocay et al.
patent: 3384694 (1968-05-01), Nakayama et al.
patent: 3404204 (1968-10-01), Nakagawa et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for spinning modacrylic fiber having high retraction and does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for spinning modacrylic fiber having high retraction and, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for spinning modacrylic fiber having high retraction and will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-618438

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.