Process for solution mining of uranium ores

Chemistry of inorganic compounds – Treating mixture to obtain metal containing compound – Radioactive metal

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

299 5, C01G 4300, E21B 4328

Patent

active

043024297

ABSTRACT:
In a process for the solution mining of a uranium ore formation using an aqueous alkaline carbonate leaching solution containing hydrogen peroxide as oxidant, the solution is passed through the ore formation in the presence of an alkylidene-1,1-diphosphonic acid. Such an acid has been found to be unique in its capability for stabilizing the peroxide against decomposition in the presence of the uranium ore.

REFERENCES:
patent: 3687627 (1972-08-01), Stalter
patent: 3740187 (1973-06-01), Kowalski
patent: 3746646 (1973-07-01), Boixader
patent: 3792903 (1974-02-01), Rhoades
patent: 3795625 (1974-03-01), Kowalski
patent: 3865435 (1975-02-01), Sareen et al.
patent: 4103963 (1978-08-01), Espenscheid et al.
patent: 4155982 (1979-05-01), Hunkin et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for solution mining of uranium ores does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for solution mining of uranium ores, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for solution mining of uranium ores will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2174605

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.