ABSTRACT:
A method of processing hydraulically mined ore slurries containing, in addition to the valuable ore, substantial quantities of contaminating argillaceous material and silica, involving initially separating the argillaceous material from the ore slurry while concomitantly concentrating said slurry to at least 65% solids content, depositing the wet concentrate thus formed on a continuous belt and conveying said wet concentrate via said belt to a beneficiation plant for further treatment.

REFERENCES:
patent: 2164052 (1939-06-01), Bullwinkel
patent: 2546247 (1951-03-01), Wolf
patent: 3204877 (1965-09-01), Barr, Jr. et al.
patent: 4044107 (1977-08-01), Houghtaling

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for sizing and desliming of ore matrix does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for sizing and desliming of ore matrix, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for sizing and desliming of ore matrix will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2046384

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.