ABSTRACT:
A process is provided for rotolining the interior surface of an oil pipe having an inner diameter of at least 2 in (5.1 cm) and no greater than 6 in (15.2 cm) and length of at least 10 ft (3 m), comprising introducing particles of rotolining composition comprising fluoropolymer and no greater than 2 wt % of metal powder into the interior of said pipe, heating the pipe to a temperature above the melting temperature of the fluoropolymer, rotating the pipe around its longitudinal axis during the heating and rocking the pipe end-to-end thereof during the rotating so as to distribute the composition over the entire interior of the pipe, the combination of heating and distributing causing the particles to melt and coalesce to form a rotolining on the pipe over its entire interior.
REFERENCES:
patent: 4312961 (1982-01-01), Winegar et al.
patent: 5397831 (1995-03-01), Saito et al.
patent: 5760151 (1998-06-01), Aten et al.
patent: 5981673 (1999-11-01), DeSimone et al.
patent: 6287632 (2001-09-01), Nishio et al.
patent: 6632902 (2003-10-01), Lahijani
patent: 2004/0204536 (2004-10-01), Miyatani et al.
patent: 2005/0173012 (2005-08-01), McKeen
patent: 0 266 668 (1992-01-01), None
patent: 1 031 384 (2000-08-01), None
patent: 1 188 808 (2002-03-01), None
patent: 03-207474 (1991-09-01), None
patent: 2904593 (1992-09-01), None
John Scheirs, Modern Fluoropolymer, (1997), pp. 314-315, John Wiley & Sons, England.
E.I. Du Pont de Nemours and Company
Fletcher, III William Phillip
LandOfFree
Process for rotolining the interior surface of an oil pipe does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for rotolining the interior surface of an oil pipe, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for rotolining the interior surface of an oil pipe will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2734401