ABSTRACT:
A cobalt base, high temperature brazing alloy having a composition, by weight of:
REFERENCES:
patent: 3632319 (1972-01-01), Hoppin et al.
patent: 4249963 (1981-02-01), Young
patent: 4285459 (1981-08-01), Baladjanian et al.
patent: 4830934 (1989-05-01), Ferrigno et al.
Beltran Adrian M.
Kreischer Charles H.
General Electric Company
Wyszomierski George
LandOfFree
Process for repairing co-based superalloy using co-based brazing does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for repairing co-based superalloy using co-based brazing, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for repairing co-based superalloy using co-based brazing will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1246110