Process for removing polyacetal binder from molded ceramic green

Plastic and nonmetallic article shaping or treating: processes – Forming articles by uniting randomly associated particles

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

264 63, 26421111, 2643282, 264344, 419 36, 419 38, 419 41, 419 44, 419 65, C04B 3302

Patent

active

050808460

ABSTRACT:
A polyacetal binder is removed from an extruded or injection molded ceramic green body in less than 25 hours by a variable heating rate schedule in which the heating rate is reduced when the temperature of the green body reaches the point at which isothermal degradation of the polyacetal binder can take place and wherein at least 80 wt. % of the binder can be removed. In air, the isothermal removal of the binder can take place within the range of 160.degree.-220.degree. C. while in nitrogen the range is from about 300.degree.-360.degree. C.

REFERENCES:
patent: 4624812 (1986-11-01), Farrow et al.
patent: 4664883 (1987-05-01), Melody et al.
patent: 4784812 (1988-11-01), Saitoh et al.
patent: 4795598 (1989-01-01), Billiet

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for removing polyacetal binder from molded ceramic green does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for removing polyacetal binder from molded ceramic green, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for removing polyacetal binder from molded ceramic green will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-539838

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.