This invention covers a process for reducing the sulfur content of coal and coal char and the ignition temperature of coal char. Coal is converted into char at temperatures not in excess of about 1600.degree. F. The char is introduced into a caustic system which is maintained at a temperature between about 500.degree. F. to about 750.degree. F. Intimate contact is maintained between the caustic and the char for a period of about 2 to 30 minutes to leach the sulfur from the char. The desulfurized char is thereafter separated from the caustic and washed.

REFERENCES:
patent: 2878163 (1959-03-01), Hutchings
"The Effect of Molten Caustic on Pyritic Sulfur in Bituminous Coal" by P. X. Masciantonio from "Fuel", vol. 44, pp. 269-275-London.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for reducing the sulfur content of coal and coal char an does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for reducing the sulfur content of coal and coal char an, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for reducing the sulfur content of coal and coal char an will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1853449

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.