Chemistry of inorganic compounds – Treating mixture to obtain metal containing compound – Alkaline earth metal
Patent
1981-06-11
1983-08-16
Straub, Gary P.
Chemistry of inorganic compounds
Treating mixture to obtain metal containing compound
Alkaline earth metal
423170, 423 15, 423 18, 423 20, 423319, 423321R, 423555, 106109, C01F 1146, C01F 512, C01B 2516, C01G 4300
Patent
active
043991106
ABSTRACT:
The level of radioactivity in gypsum produced from phosphate rock can be reduced by adding to the slurry of acid and phosphate rock in the conventional process for producing phosphoric acid a combination of concentrated nitric acid or hydrochloric acid and an ammonium salt, especially ammonium nitrate or ammonium phosphate, before the precipitation of the calcium sulfate.
REFERENCES:
patent: T970007 (1978-05-01), McCullough et al.
patent: 1856187 (1932-05-01), Johnson
patent: 1936316 (1933-11-01), Wadsted
patent: 3382035 (1968-05-01), Slater
patent: 3880980 (1975-04-01), Wamser
patent: 3919395 (1975-11-01), Hauge
patent: 4012491 (1977-03-01), Hauge
patent: 4073635 (1978-02-01), Suppanen
patent: 4180545 (1979-12-01), McCullough et al.
patent: 4301122 (1981-11-01), Johnson
patent: 4311677 (1982-01-01), Geruwda et al.
patent: 4328193 (1982-05-01), Larson
patent: 4353877 (1982-10-01), Rendall
Chemische Werke Huls Aktiengesellschaft
Straub Gary P.
LandOfFree
Process for reducing the radioactivity of calcium sulfate prepar does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for reducing the radioactivity of calcium sulfate prepar, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for reducing the radioactivity of calcium sulfate prepar will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-814309