ABSTRACT:
Freshly mined phosphate rock is subjected to screen classification in at least two stages. Only coarse grained phosphate rock with a grain size over 2 mm from the last screen classification step is fed to a plain-roller grinding mill. The rollers of the grinding mill run at different peripheral speeds, so that the grains are ground by radial and tangential forces. This produces a fine grained phosphate rock whose natural moisture content is advantageous when further processed to phosphoric acid by means of sulphuric acid.
REFERENCES:
patent: 364984 (1887-06-01), Barnard
patent: 1349221 (1920-08-01), Nolen
patent: 2174116 (1939-09-01), Bilocq
patent: 2343270 (1944-03-01), Agnew
patent: 2987263 (1961-06-01), Senn
Hoffmann Egbert
Wengeler Wilhelm
Custer, Jr. Granville Y.
Fraser Malcolm W.
Uhde GmbH
LandOfFree
Process for reducing the grain size of phosphate rock does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for reducing the grain size of phosphate rock, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for reducing the grain size of phosphate rock will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2084486