Metal fusion bonding – Process – Plural filler applying
Patent
1976-10-20
1977-09-20
Smith, Al Lawrence
Metal fusion bonding
Process
Plural filler applying
219 61, 219137WM, 228119, B23K 904
Patent
active
040491862
ABSTRACT:
The stress corrosion tendency of a welded pipe in service in a nuclear reactor water line is reduced by applying to the outside of the pipe a secondary weld bridging the primary weld of the joint beyond the axial extremities of the primary weld heat affected zone and particularly that part of the zone at the inner surface of the pipe.
REFERENCES:
patent: 2249723 (1941-07-01), Orr
patent: 2280150 (1942-04-01), Hasse
patent: 2963129 (1960-12-01), Eberle
patent: 3139511 (1964-06-01), Kudelko
patent: 3555236 (1971-01-01), Hayashi
Chrenko Richard M.
Hanneman Rodney E.
Kittle Donald B.
Cohen Joseph T.
General Electric Company
Godici Nicholas P.
Smith Al Lawrence
Squillaro Jerome C.
LandOfFree
Process for reducing stress corrosion in a weld by applying an o does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for reducing stress corrosion in a weld by applying an o, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for reducing stress corrosion in a weld by applying an o will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-667311