ABSTRACT:
Occluded acidity in particulate explosives is removed by slurrying the particles in an inert liquid and subjecting the slurry to wet-grinding. The inert liquid may include an alkaline salt at or near saturation. Separation of the ground explosive particles from the liquid phase results in a ground explosive material with much reduced acidity.

REFERENCES:
patent: 2204059 (1940-06-01), Acken
patent: 3239502 (1966-03-01), Lee et al.
patent: 3351585 (1967-11-01), Lee et al.
patent: 3600477 (1971-08-01), Friedel et al.
patent: 3770721 (1973-11-01), Robbins et al.
patent: 4156593 (1979-05-01), Tarpley, Jr.
patent: 4572439 (1986-02-01), Pitzer
patent: 4767064 (1988-08-01), Resch

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for reducing acidity of unrecrystallized explosives by w does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for reducing acidity of unrecrystallized explosives by w, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for reducing acidity of unrecrystallized explosives by w will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1021379

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.