Specialized metallurgical processes – compositions for use therei – Processes – Free metal or alloy reductant contains magnesium
Patent
1978-05-26
1979-02-06
Ozaki, G.
Specialized metallurgical processes, compositions for use therei
Processes
Free metal or alloy reductant contains magnesium
75 48, 75 63, 75 82, 75119, C22B 2304, C22B 704
Patent
active
041382498
ABSTRACT:
Disclosed is a method for recovering valuable metals from scrap including the steps of melting the initial scrap feed, carburizing the melt, solidifying the carburized melt, and recovering the valuable metals from the resulting material by ammoniacal leaching thereof.
REFERENCES:
patent: 3649487 (1972-03-01), Aue et al.
patent: 3753686 (1973-08-01), Wilder et al.
patent: 3788841 (1974-01-01), Agarwal et al.
patent: 3849269 (1974-11-01), Hartwig et al.
patent: 3880651 (1975-04-01), Queneau et al.
patent: 3967957 (1976-07-01), Fonseca
patent: 3975190 (1976-08-01), Van der Meulen et al.
Blaker Barry R.
Cabot Corporation
Chaletsky Lawrence A.
Ozaki G.
Schuman Jack
LandOfFree
Process for recovering valuable metals from superalloy scrap does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for recovering valuable metals from superalloy scrap, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for recovering valuable metals from superalloy scrap will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-889755