ABSTRACT:
A process for the production of a varistor material having a nonlinear index (.alpha.) of at least 20, which comprises adding a manganese compound to zinc oxide; heating the obtained mixture in the form of a powder in the atomosphere at 1050.degree. to 1150.degree. C.; grinding the material to give a particle size of 150 mesh or below; molding the powder into a desired shape; and sintering the same at 1200.degree. to 1350.degree. C.; is disclosed.

REFERENCES:
patent: 5039452 (1991-08-01), Thompson et al.
patent: 5039971 (1991-08-01), Imai et al.
Chemical Abstracts, vol. 85, No. 12 (9/20/76), p. 571, Abstract No. 86214n, Columbus, Ohio.
Chemical Abstracts, vol. 84, No. 12, (3/22/76), p. 655, Abstract No. 83245s, Columbus, Ohio.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for production of varistor material does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for production of varistor material, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for production of varistor material will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1508239

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.