ABSTRACT:
A process of producing a styrene polymer molding which comprises heat treating a molding of a crystalline styrene polymer having mainly a syndiotactic configuration and having a crystallinity of at least 10% as determined by X-ray diffraction analysis. The heat treating is carried out at a temperature of 150.degree.to 250.degree. C. for 20 seconds to 90 minutes.

REFERENCES:
patent: 3009206 (1961-11-01), Salyer et al.
patent: 4680353 (1987-07-01), Ishihara et al.
patent: 4824629 (1989-04-01), Seitz et al.
Neilsen, Mechanical Properties of Polymers . . ., Marcel Dekker, Inc. N.Y., N.Y. (1974) pp. 54-55.
Ishihara et al, Macromolecules, 1986, 19, 2464-2465.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for production of styrene-based polymer moldings does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for production of styrene-based polymer moldings, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for production of styrene-based polymer moldings will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1414044

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.