A process for the production of a phenolic resin modified with a liquid polybutadiene being useful as an impregnating varnish in the production of a copper-clad laminate for a printed circuit, which comprises preparing an adduct of a liquid polybutadiene having a number average molecular weight of 150 to 5,000 with an .alpha., .beta.-unsaturated dicarboxylic acid or its anhydride, subjecting the adduct to an addition reaction with one or plurality of phenols in the presence of an acid catalyst to obtain a composition and reacting the composition with formaldehyde in the presence of a basic catalyst.

REFERENCES:
patent: 3887641 (1975-06-01), Tsuchiya et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for production of phenolic resin modified with liquid po does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for production of phenolic resin modified with liquid po, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for production of phenolic resin modified with liquid po will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-653628

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.