Process for producing stereoregular polymers having a narrow mol

Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – Mixing of two or more solid polymers; mixing of solid...

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

526124, 526351, 526901, C08F 234, C08F 1006

Patent

active

050934155

ABSTRACT:
Stereoregular polymers having a molecular weight distribution of less than 5.0 and an isotactic index in excess of 96 percent are produced by polymerizing an alpha-olefin having 3 to 8 carbon atoms in a low pressure gas phase fluid bed process at a temperature in excess of 80.degree. C. employing a heat stable catalyst system comprising (a) a solid catalyst component containing magnesium, titanium, halide and a polycarboxylic acid ester containing two coplanar ester groups attached to adjacent carbon atoms, as inside electron donor, (b) an organoaluminum cocatalyst, and (c) a silicon compound containing a silicon-oxygen-carbon linkage, as outside electron donor.

REFERENCES:
patent: 4535068 (1985-08-01), Job
patent: 4611038 (1986-09-01), Brun et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for producing stereoregular polymers having a narrow mol does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for producing stereoregular polymers having a narrow mol, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for producing stereoregular polymers having a narrow mol will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-272945

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.