ABSTRACT:
In a process for the production of steel with low hydrogen content in a through-blowing oxygen converter with nozzles arranged below the bath surface in the refractory brick lining, the nozzles composed of concentric pipes for introducing oxygen sheathed by a protective medium, and with an oxygen lance projecting into the converter opening, for a hydrogen content as low as possible of about 2 ppm maximum, at least half the total quantity of oxygen is blown onto the bath and the nozzles arranged below the bath surface are temporarily operated toward the termination of refining with a hydrogen-free gas.

REFERENCES:
patent: 3854932 (1974-12-01), Bishop
patent: 3953199 (1976-04-01), Michaelis
patent: 4089677 (1978-05-01), Spenceley
patent: 4178173 (1979-12-01), Gorges

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for producing steel with low hydrogen content in a throu does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for producing steel with low hydrogen content in a throu, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for producing steel with low hydrogen content in a throu will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1340934

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.