ABSTRACT:
A plate group is formed of positive and negative plates and separators formed mostly of glass fibers of a diameter not thicker than 1.0 micron and is inserted into a container. Then, a sulfuric acid electrolyte of a concentration of a viscosity increasing agent of 0 to 3.0% by weight is first poured in an amount smaller than the total pore volume of the plate group and a sulfuric acid electrolyte of a concentration of the viscosity increasing agent higher than in the above poured sulfuric acid electrolyte is then poured in so that the total poured amount may be the same as or larger than the total pore volume of the plate group.
The sealed lead-acid battery obtained as mentioned above has an excellent discharge characteristic and gas recombining performance, is low in the internal resistance, is long in the service life and does not leak the electrolyte.

REFERENCES:
patent: 3172782 (1965-03-01), Joche
patent: 3402077 (1968-09-01), Kida et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for producing sealed lead-acid battery does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for producing sealed lead-acid battery, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for producing sealed lead-acid battery will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1433721

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.