Process for producing perlite microspheres

Compositions: coating or plastic – Materials or ingredients

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

106DIG2, 106 40R, 252378P, C09C 128, C04B 3122

Patent

active

039619788

ABSTRACT:
Perlite reduced to a particle size of less than 200 mesh in a binder of aqueous sodium ligno-sulfonate is expanded while suspended in a gaseous medium in a fluidized state at temperatures ranging from 1800.degree. to 2200.degree.F. for a period of 30 to 60 seconds. The resultant microspheres have excellent physical properties and are suited to use as fillers for resins.

REFERENCES:
patent: 2977240 (1961-03-01), Houston
patent: 3458332 (1969-07-01), Alford et al.
patent: 3752685 (1973-08-01), Honda et al.
patent: 3810773 (1974-05-01), Shannon

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for producing perlite microspheres does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for producing perlite microspheres, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for producing perlite microspheres will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1095988

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.