ABSTRACT:
A process for producing a modified ultrahigh-molecular-weight polyolefin composition, which comprises mixing a powder of an ultrahigh-molecular-weight polyolefin (A) having an intrinsic viscosity of at least 5 dl/g, a flowability improver (B) having a melting point lower than the melting point of the ultrahigh-molecular-weight polyolefin (A), a monomer (C) having an olefinically unsaturated bond and a radical initiator (D) with stirring at the melting point of the flowability improver (B) or a higher temperature but below the melting point of the ultrahigh-molecular-weight polyolefin (A), and then melt-kneading them at the melting point of the ultrahigh-molecular-weight polyolefin (A) or a higher temperature to react the monomer (C) with the ultrahigh-molecular-weight polyolefin (A).
Harazoe Hirofumi
Ohori Yoshiji
Lorin Hubert C.
Mitsui Petrochemical Industries Ltd.
LandOfFree
Process for producing modified ultrahigh-molecular-weight polyol does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for producing modified ultrahigh-molecular-weight polyol, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for producing modified ultrahigh-molecular-weight polyol will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-989246