Synthetic resins or natural rubbers -- part of the class 520 ser
Synthetic resins
Mixing of two or more solid polymers; mixing of solid...
C525S263000, C525S264000, C525S273000, C525S277000, C525S284000, C525S285000, C525S286000
Reexamination Certificate
active
06875823
ABSTRACT:
There is provided a process for producing a modified polyolefin resin, which comprises the steps of:(1) blending at least the following components (A) to (D) to produce a blend:(A) 100 parts by weight of a polyolefin resin,(B) from 0.1 to 20 parts by weight of a compound having an epoxy group and an unsaturated bond,(C) from 0.01 to 20 parts by weight of an organic peroxide having a decomposition temperature of from 50 to 115° C., at which temperature a half-life thereof is 1 minute, and(D) from 0 to 20 parts by weight of an organic peroxide having a decomposition temperature of from 150 to 200° C., at which temperature a half-life thereof is 1 minute, and(2) melt-kneading said blend to produce a modified polyolefin resin.
REFERENCES:
patent: 6569950 (2003-05-01), Kitano et al.
patent: 5-209025 (1993-08-01), None
patent: 2001-122931 (2001-05-01), None
Kondo Shin-ichi
Sanada Takashi
Rabago Roberto
Sumitomo Chemical Company Limited
LandOfFree
Process for producing modified polyolefin resin does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for producing modified polyolefin resin, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for producing modified polyolefin resin will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3395884