ABSTRACT:
5 to 50 wt. % of an alkaline flux such as sodium carbonate, sodium hydroxide, potassium carbonate and potassium hydroxide is added and mixed to aluminum smelting dust. The mixture is roasted, the roasted mixture is acid-leached with mineral acids such as sulfuric acid, hydrochloric acid and nitric acid, and then gallium is preferentially extracted at a high yield compared to other components of the dust.
REFERENCES:
patent: 4252777 (1981-02-01), McDowell et al.
Era Akio
Ikeda Hidetsuga
Matsui Shingo
Mitsui Aluminium Co., Ltd.
Stoll Robert L.
LandOfFree
Process for producing gallium-containing solution from aluminum does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for producing gallium-containing solution from aluminum , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for producing gallium-containing solution from aluminum will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2219964