ABSTRACT:
In a process for producing a vulcanizable rubber composition containing silica and having a low content of carbon black, at least a silica-based reinforcing filler and ad least a silane-based coupling agent are added to and intimately mixed with other ingredients of the composition in subsequent steps, at a temperature of from 165.degree. and 180.degree. C. and between 1100 and 160.degree. C. respectively. The rubber composition so obtained has an improved silica dispersion, constant physico-mechanical characteristics and a better drawability and is particularly suitable for the manufacture of treads for tires with low rolling resistance.
REFERENCES:
patent: 5227425 (1993-07-01), Rauline
Joseph Christa
Nahmias Marco
Schrafft Robert
Cain Edward J.
Pirelli Coordinamento Pneumatici S.p.A.
LandOfFree
Process for producing a vulcanizable rubber composition with sil does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for producing a vulcanizable rubber composition with sil, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for producing a vulcanizable rubber composition with sil will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1375890