Crude phosphate is leached with nitric acid to produce an acid slurry, which is thereafter neutralized with ammonia in two successive stages while simultaneously cooling it and adding acid, part of the crude phosphate phosphorus being replaced with phosphoric acid added to the slurry to be neutralized, and in such a manner that at maximum 40% of the phosphoric acid is fed to the first neutralization stage and the rest is fed to the second neutralization stage, whereby the acidity of the slurry is adjusted to pH 2.5 - 4.5 during the first and to pH 5.0 - 6.0 during the second neutralization stage.

REFERENCES:
patent: 3026192 (1962-03-01), Tapin
patent: 3249421 (1966-05-01), Bigot et al.
patent: 3416910 (1968-12-01), Legal, Jr.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for producing a slurry suitable for the manufacture of a does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for producing a slurry suitable for the manufacture of a, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for producing a slurry suitable for the manufacture of a will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-522582

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.