ABSTRACT:
In this process there is determined, as a function of the conditions of the environment or other conditions, the distance from the surface of the bath at which the temperature of the zinc coating on the sheet or strip is in the range in which the zinc passes through a liquid-solid transitory state which is characterized by its friability. There is exerted at this point a mechanical action on at least one of the sides of the sheet or strip so as to completely remove away the whole of the non-alloyed zinc and allow to remain only a thin iron-zinc alloy coating whose thickness is between 1 and 2 .mu.m, which represents an amount of alloy of between 7 and 15 g/m.sup.2.
REFERENCES:
patent: 1252363 (1918-01-01), Roberts
patent: 3112213 (1963-11-01), Lusa
patent: 3260577 (1966-07-01), Mayhew
patent: 4120997 (1978-10-01), Franks et al.
patent: 4137347 (1979-01-01), Graft
patent: 4171394 (1979-10-01), Patil et al.
Foret Michel
Schoeps Bernard
Kendall Ralph S.
Laminoirs de Strasbourg
LandOfFree
Process for producing a sheet or strip which is lightly galvaniz does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for producing a sheet or strip which is lightly galvaniz, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for producing a sheet or strip which is lightly galvaniz will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-335636