ABSTRACT:
A process for producing a low gloss thermoplastic resin which comprises polymerizing in two steps from 20 to 70 parts by weight of a butadiene polymer, at least 70% by weight of which is constituted by butadiene, with from 30 to 80 parts by weight of a total of from 15 to 40% by weight of a vinyl cyanide monomer and from 60 to 85% by weight of an aromatic vinyl monomer, characterized in that for the polymerization of the first step, the butadiene polymer, the vinyl cyanide monomer and the aromatic vinyl monomer were charged in amounts corresponding to from 20 to 80% by weight of the entire butadiene polymer, from 20 to 80% by weight of the entire vinyl cyanide monomer and from 20 to 80% by weight of the entire aromatic vinyl monomer, respectively, and after the completion of the polymerization of the first step, the rest of the butadiene polymer, the vinyl cyanide monomer and the aromatic vinyl monomer were charged for the polymerization of the second step.
REFERENCES:
patent: 3442979 (1969-05-01), Ott et al.
patent: 3663656 (1972-05-01), Ford et al.
patent: 4012462 (1977-03-01), Chaudhary
patent: 4221883 (1980-09-01), Mott et al.
patent: 4703090 (1987-10-01), Ferraresi et al.
Kishida Kazuo
Mikami Yoshiyuki
Toyooka Yutaka
Briggs Sr. Wilbert J.
Mitsubishi Rayon Company Limited
LandOfFree
Process for producing a low gloss thermoplastic resin does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for producing a low gloss thermoplastic resin, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for producing a low gloss thermoplastic resin will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-626622