ABSTRACT:
A process for producing a coal-water slurry having a high coal concentration (generally 60 to 80% by weight or more) and a lower viscosity, at a lower cost and with a smaller amount of dispersing agent added is provided, which process is directed to a process for producing a high concentration coal-water slurry by feeding coal, water and a dispersing agent into a wet, continuous ball mill and wet-milling them, characterized by feeding the dispersing agent in a multi-stage manner along the milling direction of coal within the ball mill.
REFERENCES:
patent: 2620987 (1952-12-01), Kennedy
patent: 2754067 (1956-07-01), Klugh
patent: 3117733 (1964-01-01), Cleeman
patent: 3459380 (1969-08-01), Kartman
patent: 3993252 (1976-11-01), Ito et al.
patent: 4288166 (1981-09-01), Nakabayashi et al.
patent: 4500041 (1985-02-01), Nakaoji et al.
Kaku Hiroyuki
Kikkawa Hirofumi
Meguri Nobuyasu
Murata Masayasu
Nishimura Yasuyuki
Babcock-Hitachi Kabushiki Kaisha
Rosenbaum Mark
LandOfFree
Process for producing a coal-water slurry does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for producing a coal-water slurry, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for producing a coal-water slurry will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-762253