Process for preparing prilled porous ammonium nitrate

Plastic and nonmetallic article shaping or treating: processes – Formation of solid particulate material directly from molten... – By extrusion spraying or gravity fall through orifice

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

149 46, 264DIG51, 264 14, B01J 204

Patent

active

039668533

ABSTRACT:
A prilled ammonium nitrate containing 2 to 5 percent by weight water obtained by prilling an aqueous solution of 93 to 98 percent by weight ammonium nitrate is dried by: lowering the drying temperature of the ammonium nitrate to a temperature less than the III--IV crystalline transition temperature of ammonium nitrate at least once when the water content of the prilled ammonium nitrate is 0.3 to 1.5 percent by weight in the drying step; further drying at a temperature higher than the III--IV transition temperature; and adding an anti-caking agent to the dried prilled ammonium nitrate. The dried, prilled ammonium nitrate obtained is useful as an ammonium nitrate fuel oil explosive.

REFERENCES:
patent: 2382298 (1945-08-01), Datin
patent: 2887724 (1959-05-01), Bettes, Jr.
patent: 3127249 (1964-03-01), Cuthbert

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for preparing prilled porous ammonium nitrate does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for preparing prilled porous ammonium nitrate, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for preparing prilled porous ammonium nitrate will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1278158

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.