ABSTRACT:
A precipitation procedure for preparing pulverulent coating compositions of high molecular weights by post condensation and based on polyamides having at least ten aliphatically bound carbon atoms per carbonamide group. The starting materials are uncontrolled polyamides having a relative solution viscosity of between 1.7 and 2.0 (measured in 0.5% meta cresol solution at 25.degree. C.) and contain not more than 0.2% by weight of phosphoric acid. After the cooling stage of the precipitation step of the polyamides, from 0.3 to 1.2% by weight of phosphoric acid referred to the polyamide are dispersed in the suspension prior to the precipitation in the solution or after the precipitation stage.

REFERENCES:
patent: 4273919 (1981-06-01), Feldmann et al.
patent: 4334056 (1982-06-01), Meyer et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for preparing polyamide-based, pulverulent coating compo does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for preparing polyamide-based, pulverulent coating compo, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for preparing polyamide-based, pulverulent coating compo will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-23091

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.