Process for preparing high strength polyamide and polyester fila

Plastic and nonmetallic article shaping or treating: processes – Forming continuous or indefinite length work – Shaping by extrusion

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

264176F, D01D 512

Patent

active

041138210

ABSTRACT:
Preparation of improved yarns from synthetic linear polymer filaments by melt spinning followed by substantially immediately heating said filaments above their second order transition temperature and drawing said filaments substantially instantly at a temperature in the range of from about above their second order transition temperature to within about 5.degree. C. of their melting point, said heating being preceded by pretensioning of said filaments at a constant tension level greater than about 0.005 gram per denier and less than a tension level required to draw said filaments.

REFERENCES:
patent: 3216187 (1965-11-01), Chantry et al.
patent: 3361859 (1968-01-01), Cengato
patent: 3715421 (1973-02-01), Martin et al.
patent: 3936253 (1976-02-01), Fisher et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for preparing high strength polyamide and polyester fila does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for preparing high strength polyamide and polyester fila, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for preparing high strength polyamide and polyester fila will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2384400

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.